Effects of Nb Element Addition on the Short Range Order Characteristics of Nickel-Based Superalloys


Mehrabov Ə., Akdeniz M. V.

V-th International Scientific-Practical Conference on “Modern problems of Physics of Metals”, Baku, Azerbaijan, 10 - 11 June 2016, pp.48-52, (Full Text)