Microstructural Evolution of γ'-Ni3Al Precipitates Affecting Mechanical Properties of Nickel-based Superalloys


Mehrabov Ə., Akdeniz M. V.

TMS 2020 Annual Meeting & Exhibition, California, United States Of America, 23 - 27 February 2020, pp.324, (Summary Text)